Abu | Bayanai |
Launi | m |
Yawan cakude | 2:1:0.3 |
Fesa shafi | 2-3 yadudduka, 40-60um |
Tazarar lokaci (20°) | Minti 5-10 |
Lokacin bushewa | Surface bushe minti 45, goge 15 hours. |
Lokacin samuwa (20°) | 2-4 hours |
Fesa da amfani da kayan aiki | Geocentric spray gun (kwalba na sama) 1.2-1.5mm; 3-5kg/cm² |
Gun fesa gun (ƙananan kwalban) 1.4-1.7mm;3-5kg/cm² | |
Ka'idar adadin fenti | 2-3 yadudduka kamar 3-5㎡/L |
Rayuwar ajiya | Ajiye fiye da shekaru biyu ajiye a cikin akwati na asali. |
. Yana ba da damar ingantaccen gyare-gyare cikin sauri
.Yana rage lahanin fenti
. Canjin kayan aikin bushewa
.Ingantacciyar amfani da kayan aiki
1, Ya shafi ƙasa sosai da kuma tsabtace tsaka-tsakin fenti, fenti na asali ko saman fenti na 2K.Kuma kayan tushe mai laushi tare da insulating Layer.
2, Ana iya amfani da shi don feshin wasu sabbin motoci ko gyaran tsofaffin motoci.
Tsohuwar fim ɗin fenti wanda aka taurare kuma an goge shi, saman ya kamata ya bushe kuma ba shi da ƙazanta irin su maiko.
1.Spray har zuwa yiwu, lokuta na musamman na iya zama shafi na buroshi;
2.The Paint dole ne a ko'ina gauraye a lokacin gina, da kuma Paint ya kamata a diluted da musamman ƙarfi ga danko da ake bukata domin gina.
3.A lokacin gina, da surface ya kamata a bushe da kuma tsabtace da ƙura.
4.Spray 2-3 yadudduka, na iya zama polishing bayan 15 hours.
1.Base zafin jiki neba kasa da 5 ° C ba, da dangi zafi na 85% (zazzabi da dangi zafi ya kamata a auna kusa da tushe abu), hazo, ruwan sama, dusar ƙanƙara, iska da ruwan sama ne tsananin haramta yi.
2.Kafin fenti,tsaftace rufin rufindon guje wa kazanta da mai.
3.A samfurin za a iya fesa, ana bada shawara don fesa tare da kayan aiki na musamman.A bututun ƙarfe diamita ne 1.2-1.5mm, da fim kauri ne 40-60um.